New superalloy could cut carbon emissions from power plants

As the world looks for ways to cut greenhouse gas emissions, researchers from Sandia National Laboratories have shown that a new 3D-printed superalloy could help power plants generate more electricity while producing less carbon.

from Energy & Green Tech News - Energy Sciences News, Green Tech, Energy, Energy Science https://ift.tt/wurThe0